소개
In the present research, the high temperature oxidation and high temperature corrosion (simulated boiler conditions) behavior of Wire Arc sprayed Ni-based coating (Ni-5Al and Ni-20Cr) on commonly used T11 and Gr A1 boiler steels was studied at 900 degree C for 50 cycles. Each cycle consisted of 1 hour heating at 900 degree C followed by 20 min. of cooling in air at room temperature.